Hydrogenation of Anthracene and Dehydrogenation of Perhydroanthracene on Pt/C Catalysts


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The hydrogenation of anthracene on a heterogeneous catalyst containing 3 wt % Pt/C (Aldrich) at 215, 245, and 280°C and the pressures of 40 and 90 atm is studied. The hydrogenation of anthracene to a completely hydrogenated product is considered in detail. The final product (perhydroanthracene) consists of five conformational isomers with total selectivity of more than 99%. The ratio of perhydroanthracene isomers in the end product is shown to be determined by the conditions (P, T) of hydrogenation. The rate of hydrogenation is found to slow upon an increase in the degree of benzene ring saturation. A mixture of perhydroanthracene isomers is dehydrogenated in an autoclave at 260−325°C on 3 wt % Pt/C catalyst (Aldrich) and in a flow reactor at 300–360°C on 3 wt% Pt/Sibunit catalyst. The reactivity of perhydroanthracene isomers in dehydrogenation is shown to differ.

作者简介

A. Kalenchuk

Department of Chemistry; Zelinsky Institute of Organic Chemistry

编辑信件的主要联系方式.
Email: akalenchuk@yandex.ru
俄罗斯联邦, Moscow, 119991; Moscow, 119991

A. Koklin

Zelinsky Institute of Organic Chemistry

Email: akalenchuk@yandex.ru
俄罗斯联邦, Moscow, 119991

V. Bogdan

Department of Chemistry; Zelinsky Institute of Organic Chemistry

Email: akalenchuk@yandex.ru
俄罗斯联邦, Moscow, 119991; Moscow, 119991

V. Lunin

Department of Chemistry

Email: akalenchuk@yandex.ru
俄罗斯联邦, Moscow, 119991

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018