Hydrogenation of Anthracene and Dehydrogenation of Perhydroanthracene on Pt/C Catalysts


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The hydrogenation of anthracene on a heterogeneous catalyst containing 3 wt % Pt/C (Aldrich) at 215, 245, and 280°C and the pressures of 40 and 90 atm is studied. The hydrogenation of anthracene to a completely hydrogenated product is considered in detail. The final product (perhydroanthracene) consists of five conformational isomers with total selectivity of more than 99%. The ratio of perhydroanthracene isomers in the end product is shown to be determined by the conditions (P, T) of hydrogenation. The rate of hydrogenation is found to slow upon an increase in the degree of benzene ring saturation. A mixture of perhydroanthracene isomers is dehydrogenated in an autoclave at 260−325°C on 3 wt % Pt/C catalyst (Aldrich) and in a flow reactor at 300–360°C on 3 wt% Pt/Sibunit catalyst. The reactivity of perhydroanthracene isomers in dehydrogenation is shown to differ.

Sobre autores

A. Kalenchuk

Department of Chemistry; Zelinsky Institute of Organic Chemistry

Autor responsável pela correspondência
Email: akalenchuk@yandex.ru
Rússia, Moscow, 119991; Moscow, 119991

A. Koklin

Zelinsky Institute of Organic Chemistry

Email: akalenchuk@yandex.ru
Rússia, Moscow, 119991

V. Bogdan

Department of Chemistry; Zelinsky Institute of Organic Chemistry

Email: akalenchuk@yandex.ru
Rússia, Moscow, 119991; Moscow, 119991

V. Lunin

Department of Chemistry

Email: akalenchuk@yandex.ru
Rússia, Moscow, 119991

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Ltd., 2018