Characteristics of the Li+-Ion Conductivity of Li3R2(PO4)3 Crystals (R = Fe, Sc) in the Superionic State


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The characteristics of Li+-ion conductivity σdc of structural γ modifications of Li3R2(PO4)3 compounds (R = Fe, Sc) existing in the superionic state have been investigated by impedance spectroscopy. The type of structural framework [R2P3O12]3- affects the σdc value and the σdc activation enthalpy in these compounds. The ion transport activation enthalpy in γ-Li3R2(PO4)3Hσ = 0.31 ± 0.03 eV) is lower than in γ-Li3Fe2(PO4)3Hσ = 0.36 ± 0.03 eV). The conductivity of γ-Li3Fe2(PO4)3dc = 0.02 S/cm at 573 K) is twice as high as that of γ-Li3R2(PO4)3. A decrease in temperature causes a structural transformation of Li3R2(PO4)3 from the superionic γ modification (space group Pcan) through the intermediate metastable β modification (space group P21/n) into the “dielectric” α modification (space group P21/n). Upon cooling, σdc for both phosphates decreases by a factor of about 100 at the superionic TSIC transition. In Li3Fe2(PO4)3 σdc gradually decreases in the temperature range TSIC = 430–540 K, whereas in Li3R2(PO4)3 σdc undergoes a jump at TSIC = 540 ± 25 K. Possible crystallochemical factors responsible for the difference in the σdc and ΔHσ values and the thermodynamics and kinetics of the superionic transition for Li3R2(PO4)3 are discussed.

Авторлар туралы

N. Sorokin

Shubnikov Institute of Crystallography, Federal Scientific Research Centre “Crystallography and Photonics”

Хат алмасуға жауапты Автор.
Email: nsorokin1@yandex.ru
Ресей, Moscow, 119333

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2018