Improving the Chemical Purity of Fused Corundum by High-Temperature Roasting


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The chemical purity of fused corundum was demonstrated experimentally to improve after high-temperature (~1750°C) vacuum (~10–5 mm Hg) roasting. Three industrial fused corundum samples with different particle-size and impurity profiles were heat treated, after which the impurity contents decreased by an order of magnitude. The samples were practically completely purified of Na, Mg, K, Mn, Cu, and Zn whereas the Fe content decreased by 8 – 10 times. Samples were found to consist of porous granules 16 – 60 μm in size that consisted of solid microparticles of characteristic size 0.4 – 0.7 μm. The specific surface area of the granules lay in the range 2.8 – 3.3 cm2/g.

Авторлар туралы

G. Belyaev

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: 666zhuk@ihed.ras.ru
Ресей, Moscow

M. Vlaskin

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: 666zhuk@ihed.ras.ru
Ресей, Moscow

A. Grigorenko

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: 666zhuk@ihed.ras.ru
Ресей, Moscow

A. Zhuk

Joint Institute for High Temperatures, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: 666zhuk@ihed.ras.ru
Ресей, Moscow

I. Lipatova

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: 666zhuk@ihed.ras.ru
Ресей, Moscow

E. Shkol’nikov

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: 666zhuk@ihed.ras.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2019