Thermoelectric Properties of Bi2Te2.7Se0.3 Solid Solution with Various Grain Sizes


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The electrical conductivity (σ) and the coefficients of thermal e.m.f. (α), Holl (RH), and thermal conductivity (χ) of extruded n-Вi2Te2.7Se0.3 samples with various grain sizes are studied in the temperature range 77–300 K after extrusion and upon subsequent annealing. It is shown that annealing substantially increases σ and χ and has a little effect on α at 77 K. This indicates that at 77 K, the structural imperfections of grains play the main role in the electron and phonon scattering. There is a correlation between the degree of texture and thermoelectric properties.

Авторлар туралы

M. Tagiyev

Azerbaijan State Economic University

Хат алмасуға жауапты Автор.
Email: mail_tagiyev@mail.ru
Әзірбайжан, Baku

S. Dzhafarova

Azerbaijan State Economic University

Email: mail_tagiyev@mail.ru
Әзірбайжан, Baku

A. Ahmedova

Azerbaijan State Economic University

Email: mail_tagiyev@mail.ru
Әзірбайжан, Baku

G. Abdinova

Institute of Physics of the National Academy of Sciences of Azerbaijan

Email: mail_tagiyev@mail.ru
Әзірбайжан, Baku

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2019