Electrochemical Amorphization As a Method to Increase the Rate Capability of Crystalline Silicon Anodes for Lithium-Ion Batteries


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

Anodes manufactured from macroporous silicon have been studied. Galvanostatic cycling tests in half-cells with Li counterelectrode in a regime of charging capacity limited to Q1 = 1000 mAh/g showed that the inclusion of a modifying cycle with increased time of electrochemical lithiation into the testing schedule allowed the charge/discharge rate to be increased upon return to the initial regime. The results are interpreted in terms of a two-phase model with a sharp a-LixSi/c-Si interface. The insertion of a large amount of lithium during the modifying cycle leads to an increase in the thickness of an amorphous layer, within which the insertion and extraction of lithium in subsequent cycles proceed at a higher rate.

Об авторах

G. Li

Ioffe Physical Technical Institute, Russian Academy of Sciences

Email: east@mail.ioffe.ru
Россия, St. Petersburg, 194021

E. Astrova

Ioffe Physical Technical Institute, Russian Academy of Sciences

Автор, ответственный за переписку.
Email: east@mail.ioffe.ru
Россия, St. Petersburg, 194021

A. Rumyantsev

Ioffe Physical Technical Institute, Russian Academy of Sciences

Email: east@mail.ioffe.ru
Россия, St. Petersburg, 194021

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2019

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).