Dependence of the optimum parameters of femtosecond laser annealing of lead zirconate titanate films on their thickness


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The optimum parameters of laser annealing (crystallization) induced by repetitive pulses with a pulse duration of 100 fs and a wavelength of 800 nm, which falls in the transparency region of the film and, simultaneously, in the absorption region of the substrate, have been investigated experimentally as a function of the thickness of the ferroelectric film. It has been shown that, with an increase in the thickness of the ferroelectric film by 100 nm (in the range from 300 to 600 nm), the required power density of the laser beam increases, on the average, by 0.1 MW/cm2. The optimum exposure time of the laser beam with the desired power increases nonlinearly with an increase in the thickness of the film.

Sobre autores

A. Elshin

Moscow State Technical University of Radio Engineering, Electronics, and Automation

Autor responsável pela correspondência
Email: elshin_andrew@mail.ru
Rússia, pr. Vernadskogo 78, Moscow, 119454

D. Abdullaev

Moscow State Technical University of Radio Engineering, Electronics, and Automation

Email: elshin_andrew@mail.ru
Rússia, pr. Vernadskogo 78, Moscow, 119454

E. Mishina

Moscow State Technical University of Radio Engineering, Electronics, and Automation

Email: elshin_andrew@mail.ru
Rússia, pr. Vernadskogo 78, Moscow, 119454

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Ltd., 2016