Influence of chemically active elements on the hydrogen cracking of pipe steel
- Авторлар: Golubtsov V.A.1, Ryabchikov I.V.1, Mizin V.G.2
-
Мекемелер:
- OOO NPPgroup
- Aff2
- Шығарылым: Том 46, № 3 (2016)
- Беттер: 220-223
- Бөлім: Article
- URL: https://bakhtiniada.ru/0967-0912/article/view/178621
- DOI: https://doi.org/10.3103/S0967091216030037
- ID: 178621
Дәйексөз келтіру
Аннотация
Vacuum treatment of pipe steel and the maintenance of superlow sulfur concentration (0.002%) are not enough to ensure high corrosion resistance. Hydrogen cracking of pipe steel may be prevented by if complex modifiers are used to maintain certain proportions of the active elements Al, Ca, rare-earth metals, and sulfur.