Changes in the Defect Structure of the Pd–5.3 at % In–0.5 at % Ru Alloy Subjected to Electrolytic Hydrogenation and Prolonged Relaxation
- Авторлар: Akimova O.V.1, Avdyukhina V.M.1, Shchetinin I.V.2
-
Мекемелер:
- Physical Department
- National University of Science and Technology MISIS
- Шығарылым: Том 117, № 3 (2016)
- Беттер: 275-278
- Бөлім: Structure, Phase Transformations, and Diffusion
- URL: https://bakhtiniada.ru/0031-918X/article/view/166666
- DOI: https://doi.org/10.1134/S0031918X16030017
- ID: 166666
Дәйексөз келтіру
Аннотация
Variations in the reduced integral intensities of diffraction maxima in X-ray diffraction patterns taken for the Pd–5.3 at % In–0.5 at % Ru alloy foil, which was subjected to electrolytic saturation with hydrogen and subsequent prolonged relaxation at room temperature and atmospheric pressure, have been analyzed. The degree of texture of the sample has been found to decrease substantially, and first-class defects in the alloy matrix dominate.
Негізгі сөздер
Авторлар туралы
O. Akimova
Physical Department
Хат алмасуға жауапты Автор.
Email: akimova@physics.msu.ru
Ресей, Leninskie Gory 1, build. 2, Moscow, 119991
V. Avdyukhina
Physical Department
Email: akimova@physics.msu.ru
Ресей, Leninskie Gory 1, build. 2, Moscow, 119991
I. Shchetinin
National University of Science and Technology MISIS
Email: akimova@physics.msu.ru
Ресей, Leninskii pr. 4, Moscow, 119049
Қосымша файлдар