Change in Relaxation State of Polymer Components of Wood During its High-Temperature Biorefining
- Авторлар: Akim E.L.1, Mandre Y.G.1, Pekarets A.A.1,2
-
Мекемелер:
- St. Petersburg State University of Industrial Technologies and Design
- Forest Technology Company LLC
- Шығарылым: Том 51, № 3 (2019)
- Беттер: 164-169
- Бөлім: Article
- URL: https://bakhtiniada.ru/0015-0541/article/view/235771
- DOI: https://doi.org/10.1007/s10692-019-10067-8
- ID: 235771
Дәйексөз келтіру
Аннотация
The change in relaxation state of polymer components of wood during its high-temperature biorefining and extrusion briquetting and subsequent heating at 380-450°C, i.e., above the thermal decomposition temperature of wood, is analyzed. It is demonstrated that the system can be translated into brittle state by changing the moisture content of the wood and treatment temperature and into forced plastic state by subsequent moistening, heating, and compression-shearing. Carbonization and activation of charcoal briquettes can be combined by subsequent low-temperature pyrolysis in controlled vaporgas environment conditions.
Авторлар туралы
E. Akim
St. Petersburg State University of Industrial Technologies and Design
Хат алмасуға жауапты Автор.
Email: akim-ed@mail.ru
Ресей, St. Petersburg
Yu. Mandre
St. Petersburg State University of Industrial Technologies and Design
Email: akim-ed@mail.ru
Ресей, St. Petersburg
A. Pekarets
St. Petersburg State University of Industrial Technologies and Design; Forest Technology Company LLC
Email: akim-ed@mail.ru
Ресей, St. Petersburg; Kachug, Irkutsk Region
Қосымша файлдар