Chemical Vapor Deposition of Wear-Resistant Iron-Nickel Coating onto Precision Parts of Hydraulic Systems


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Wear-resistant iron-nickel coating has been obtained by chemical vapor deposition of nickel tetracarbonyl and iron pentacarbonyl. A procedure of application of wear-resistant iron-nickel coating on precision parts has been developed where at first the surface of the item is coated with an adhesive layer of nickel coating with the thickness up to 10 μm by supplying vapor of nickel tetracarbonyl to the heated surface of the item, and then an adhesive layer of iron-nickel coating is applied by supplying a vapor mixture of nickel tetracarbonyl, iron pentacarbonyl, and carbon monoxide in a volumetric ratio of 1: 6: 15 and their combined thermal decomposition. Coatings with the required physicomechanical properties have been obtained, thus indicating the efficiency of the used approaches, increasing the wear resistance of precision items of hydraulic systems and their service life.

作者简介

L. Kozyreva

Tver State Technical University

编辑信件的主要联系方式.
Email: larisa.v.k.176@mail.ru
俄罗斯联邦, Tver, 170026

V. Kozyrev

Tver State Agricultural Academy

Email: larisa.v.k.176@mail.ru
俄罗斯联邦, Tver, 170904

N. Chupyatov

PSJC Elektromekhanika

Email: larisa.v.k.176@mail.ru
俄罗斯联邦, Rzhev, 172386

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018