Combined Elemental Synthesis of Boron and Silicon Carbides
- Autores: Nesmelov D.D.1, Vlasova E.A.1, Ordan’yan S.S.1
-
Afiliações:
- FGBOU VPO St. Petersburg State Technological Institute (Technical University)
- Edição: Volume 57, Nº 5 (2017)
- Páginas: 531-535
- Seção: Article
- URL: https://bakhtiniada.ru/1083-4877/article/view/248580
- DOI: https://doi.org/10.1007/s11148-017-0018-y
- ID: 248580
Citar
Resumo
Combined synthesis from powders of elements B, C, and Si at 1400, 1500, and 1650°C is used to prepare heterophase powders in the system SiC–B4C containing 80, 57, and 30 (mol.%) boron carbide. Powders containing only SiC and B4C phases are prepared at 1550°C from a mixture with 5% excess silicon given vibration grinding for 60 h. The powder has a unimodal particle size distribution and d50 = 3.5 μm with a volume concentration of 12% submicron particles.
Palavras-chave
Sobre autores
D. Nesmelov
FGBOU VPO St. Petersburg State Technological Institute (Technical University)
Email: ceramic-department@yandex.ru
Rússia, St. Petersburg
E. Vlasova
FGBOU VPO St. Petersburg State Technological Institute (Technical University)
Email: ceramic-department@yandex.ru
Rússia, St. Petersburg
S. Ordan’yan
FGBOU VPO St. Petersburg State Technological Institute (Technical University)
Autor responsável pela correspondência
Email: ceramic-department@yandex.ru
Rússia, St. Petersburg
Arquivos suplementares