Аннотация
Reasons are considered for crack formation in periclase-carbon, aluminopericlase-carbon and spinel-periclase-carbon refractories, and also partial effect on life of flux-cored wire and inert gas blowing intensity in enterprises smelting low-alloy, carbon, and low-silicon materials. The turnover of a steel-teeming ladle is more than 4 – 5 melts/day: the proportion of melts treated in FLU is 100%; open stream casting into a CBCM. Defining factors and the proportion of their effect on steel-teeming ladle life are evaluated from the results of this work.
Авторлар туралы
A. Kondrukevich
FGOU VO D. I. Mendeleev Russian Chemical technology University
Хат алмасуға жауапты Автор.
Email: kondrukevich@list.ru
Ресей, Moscow
D. Ryabyi
GBUZ DonGTU
Email: kondrukevich@list.ru
Украина, Lisichansk
Қосымша файлдар