Influence of electrospark discharge parameters on roughness and microabrasive wear of steel 45 surface after ESA by TiC-based electrodes


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The influence of the parameters of electrospark discharge and electrode materials for electrospark alloying using the additives of boron-containing mineral raw material on the characteristics of microgeometry and microabrasive wear of the coating surface is investigated. It is found that the longer is the electrospark duration (from 20 to 80 μs), the higher is the surface roughness. The introduction of 1–2% of boron-containing raw material improves physicochemical properties of the alloyed layer, reduces the roughness, and increases the wear resistance.

Sobre autores

S. Nikolenko

Institute of Materials Science

Autor responsável pela correspondência
Email: nikola960@mail.ru
Rússia, ul. Tikhookeanskaya 153, Khabarovsk, 680042

A. Verkhoturov

Institute of Water and Ecological Problems

Email: nikola960@mail.ru
Rússia, ul. Kim-Yu-Chena 65, Khabarovsk, 680000

N. Syui

Institute of Materials Science

Email: nikola960@mail.ru
Rússia, ul. Tikhookeanskaya 153, Khabarovsk, 680042

E. Kuz’michev

Far Eastern State Transport University

Email: nikola960@mail.ru
Rússia, ul. Serysheva 47, Khabarovsk, 680021

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Allerton Press, Inc., 2016