Hydrothermal Carbonization of Organic Components from Municipal Solid Waste
- Авторлар: Vlaskin M.S.1, Vladimirov G.N.2
-
Мекемелер:
- Joint Institute for High Temperatures, Russian Academy of Sciences
- Skolkovo Institute of Science and Technology
- Шығарылым: Том 52, № 6 (2018)
- Беттер: 996-1003
- Бөлім: Article
- URL: https://bakhtiniada.ru/0040-5795/article/view/172732
- DOI: https://doi.org/10.1134/S0040579518050421
- ID: 172732
Дәйексөз келтіру
Аннотация
The hydrothermal carbonization of organic ingredients from municipal solid waste (exemplified by apples, meat, offset paper, newsprint, birch and oak sawdust, cotton cloth, polypropylene, and polyethylene terephthalate) is studied in the temperature range 240–280°C. The yield of the solid hydrothermal carbonization product (excluding plastics) is 0.50–0.62 at 240°C, 0.46–0.54 at 260°C, and 0.37–0.46 at 280°C. The yield of the solid product in the case of polypropylene and polyethylene terephthalate is close to 1. When increasing the temperature, the carbon content of the solid product increases from 45–52% for the initial ingredients to 61–75% for the products obtained at 280°C (excluding plastics). The calorific value of the products of hydrothermal carbonization obtained from organic waste with a calorific value of 15 to 19 MJ/kg (excluding plastics) is 19–26 MJ/kg for 240°C and 21–29 MJ/kg for 280°C. The products of the hydrothermal treatment of apples and sawdust at 280°C have the highest calorific values (28–29 MJ/kg). The calorific value of plastics after hydrothermal treatment remains practically unchanged.
Негізгі сөздер
Авторлар туралы
M. Vlaskin
Joint Institute for High Temperatures, Russian Academy of Sciences
Хат алмасуға жауапты Автор.
Email: vlaskin@inbox.ru
Ресей, Moscow, 125412
G. Vladimirov
Skolkovo Institute of Science and Technology
Email: vlaskin@inbox.ru
Ресей, Skolkovo, Moscow oblast, 143025
Қосымша файлдар