Specifics of reactions of cerium sulfate and europium sulfate with hydrogen


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

Reactions of cerium sulfate and europium sulfate with hydrogen have been studied. Diagrams showing the evolution of phase composition of the polycrystalline products of reaction between europium sulfate and hydrogen are constructed. The reaction of Ce2(SO4)3 with hydrogen at 600°С consecutively yields Ce2O2S and Ce2O3 phases. At 800°С the batch is >95 mol % Ce2O3. At 480-500°С, a single-phase sample of EuSO4 is prepared; at 600-1000°С, Eu2O2S is prepared; and at 1050°С, the batch is >95 mol % Eu2O2S and up to 5 mol % Eu2O3. Atomic-force microscopy shows that europium sulfate grains, which represent agglomerates of particles 10-20 μm in size, are degraded upon reaction with hydrogen into individual ovalshaped particles sized 40-60 × 130-200 nm.

Об авторах

O. Andreev

Tyumen State University

Автор, ответственный за переписку.
Email: andreev@utmn.ru
Россия, Tyumen

Yu. Denisenko

Tyumen State University

Email: andreev@utmn.ru
Россия, Tyumen

E. Sal’nikova

Tyumen State University; Agrarian University of South Trans-Urals

Email: andreev@utmn.ru
Россия, Tyumen; Tyumen

N. Khritokhin

Tyumen State University

Email: andreev@utmn.ru
Россия, Tyumen

K. Zyryanova

Tyumen State University

Email: andreev@utmn.ru
Россия, Tyumen

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2016

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).