Influence of megaplastic deformation on the structure and hardness of Al–Cu–Mg alloy after aging


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Methods of electron microscopy and X-ray diffraction have been used to investigate structural and phase transformations in the aluminum alloy of grade A2024 (Al–4.5 Cu–1.37 Mg–0.61 Mn–0.07 Si–0.27 Fe–0.02 Zn–0.02 Ti (wt %)) after aging and deformation by shear under high quasi-static pressure. It has been shown that the combination of two-stage aging with megaplastic deformation leads to the refinement of the structure to a nanolevel and to strengthening of the alloy (to an increase in the microhardness to 3000 MPa). The values of true deformation at which the deformation-induced dissolution of the particles of the strengthening S phase occurs have been determined.

Авторлар туралы

A. Petrova

Institute of Metal Physics, Ural Branch; Ural Federal University

Хат алмасуға жауапты Автор.
Email: petrovanastya@yahoo.com
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990; ul. Mira 19, Ekaterinburg, 620002

H. Radziszewska

Tekhnical University of Lodz

Email: petrovanastya@yahoo.com
Польша, ul. Stefanovskogo 1/15, Lodz, 90-924

L. Kaczmarek

Tekhnical University of Lodz

Email: petrovanastya@yahoo.com
Польша, ul. Stefanovskogo 1/15, Lodz, 90-924

M. Klih

Tekhnical University of Lodz

Email: petrovanastya@yahoo.com
Польша, ul. Stefanovskogo 1/15, Lodz, 90-924

I. Brodova

Institute of Metal Physics, Ural Branch

Email: petrovanastya@yahoo.com
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990

M. Steglinski

Tekhnical University of Lodz

Email: petrovanastya@yahoo.com
Польша, ul. Stefanovskogo 1/15, Lodz, 90-924

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2016