Evolution of the fine structure of Pd–5.3 at % Ιn–0.5 at % Ru solid solution after hydrogenation
- Authors: Akimova O.V.1, Shchetinin I.V.2
-
Affiliations:
- Physical Department
- National University of Science and Technology MISiS
- Issue: Vol 117, No 11 (2016)
- Pages: 1119-1122
- Section: Structure, Phase Transformations, and Diffusion
- URL: https://bakhtiniada.ru/0031-918X/article/view/166414
- DOI: https://doi.org/10.1134/S0031918X16110028
- ID: 166414
Cite item
Abstract
Fine-structure parameters, such as the effective coherent domain size Dhkl and microstrain εhkl, of Ρd–5.3 at % Ιn–0.5 at % Ru alloy foil, which was subjected to electrolytic hydrogenation and subsequent prolonged (for 55000 h) relaxation, have been determined using X-ray diffraction data. The hydrogenation and subsequent relaxation of the alloy have been found to result in the refinement of coherent domains CD(hkl) and increase in the microstrains εhkl.
About the authors
O. V. Akimova
Physical Department
Author for correspondence.
Email: akimova@physics.msu.ru
Russian Federation, Leninskie Gory 1, build. 2, Moscow, 119991
I. V. Shchetinin
National University of Science and Technology MISiS
Email: akimova@physics.msu.ru
Russian Federation, Leninskii pr. 4, Moscow, 119049
Supplementary files