Intensification of Sulfide Copper-Nickel Ore Heap Leaching with Bioreagent-Oxidant Participation


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

With the aim of intensification, improving economic efficiency, and controlling sulfide ore heap bacterial leaching features and leaching regimes are studied for lean copper-nickel ore with the participation of a bioreagent-oxidant prepared by iron-oxidizing micro-organisms and concentrated adsorption immobilization in a separate reactor. Research established the ore size for heap leaching and an increase in metal extraction with an increase in bioreagent concentration. Use of the heap bioleaching technology developed for ore with a size of –10 mm containing 0.32% nickel and 0.11% copper makes it possible to increase nickel extraction into solution to 6.3–19.5% and copper to 5.8–24.2% with consumption of sulfuric acid lower by 4.4–14.6% compared with use of seeding ore with bacteria.

Авторлар туралы

Zheng Zhihong

East China Technological University (ECUST)

Хат алмасуға жауапты Автор.
Email: ecitzhzheng76@126.com
ҚХР, Nanchang

L. Krylova

National University of Science and Technology MISiS

Email: ecitzhzheng76@126.com
Ресей, Moscow

D. Ryabtsev

Engineering Center, Moscow Institute of Physics and Technology (State University)

Email: ecitzhzheng76@126.com
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media New York, 2016