Temperature dependences of the optical properties and the phase composition of vanadium dioxide films obtained by chemical vapor deposition


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

By low pressure chemical vapor deposition single-phase vanadium dioxide films containing monoclinic phase M1from vanadyl acetylacetonate vapor are obtained on monocrystalline silicon Si(100) substrates. Changes in the phase composition of the films on heating to 90 °C are studied by X-ray diffraction. It is found that in the temperature range 60-70 °C the monoclinic phase passes into tetragonal R. At higher temperatures only the tetragonal phase is observed. By reflection spectrophotometry and ellipsometry the temperature dependences of the optical properties of the films exhibiting hysteresis are determined. At wavelengths less than 600 nm the reflection spectra are almost insensitive to temperature variation. After the linear normalization the reflection and extinction coefficients are well consistent with changes in the phase composition.

作者简介

V. Shayapov

Nikolaev Institute of Inorganic Chemistry, Siberian Branch

编辑信件的主要联系方式.
Email: shayapov@niic.nsc.ru
俄罗斯联邦, Novosibirsk

L. Yakovkina

Nikolaev Institute of Inorganic Chemistry, Siberian Branch

Email: shayapov@niic.nsc.ru
俄罗斯联邦, Novosibirsk

N. Bulina

Institute of Solid State Chemistry and Mechanochemistry, Siberian Branch

Email: shayapov@niic.nsc.ru
俄罗斯联邦, Novosibirsk

N. Chernikova

Nikolaev Institute of Inorganic Chemistry, Siberian Branch

Email: shayapov@niic.nsc.ru
俄罗斯联邦, Novosibirsk

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2017