Evaluation of the maximum size of through pores in MFAS-type membranes found by different methods
- 作者: Ishkova Z.A.1, Kolunin V.S.1,2
-
隶属关系:
- Institute of the Earth’s Cryosphere, Siberian Branch
- Tyumen State Oil and Gas University
- 期: 卷 60, 编号 3 (2017)
- 页面: 434-438
- 栏目: Laboratory Techniques
- URL: https://bakhtiniada.ru/0020-4412/article/view/159792
- DOI: https://doi.org/10.1134/S0020441217030071
- ID: 159792
如何引用文章
详细
Experiments to determine the maximum size of through pores in MFAS-type membranes (Vladipor Company) were carried out in two ways: by the “bubble-point” method according to GOST (State Standard) 50516-93 and the “crystallization-onset” method. The experimental values of the pressure difference upon the appearance of bubbles in a liquid and the temperature of the crystallization onset were obtained for membranes of different brands. It was shown that the membrane thickness influences these parameters. Repeated measurements of the maximum size of through pores were performed and showed good reproducibility of the experimental data.
作者简介
Z. Ishkova
Institute of the Earth’s Cryosphere, Siberian Branch
编辑信件的主要联系方式.
Email: z.ishkova@yandex.ru
俄罗斯联邦, Tyumen, 625000
V. Kolunin
Institute of the Earth’s Cryosphere, Siberian Branch; Tyumen State Oil and Gas University
Email: z.ishkova@yandex.ru
俄罗斯联邦, Tyumen, 625000; Tyumen, 625000
补充文件